Other Products
English Name: Azodicarbonamide
Molecular Formula: C2H4O2N4
Molecular Weight: 116
Appearance: Light yellow powder
Purity: Premium grade
Package: 25 kg/bag
Physical Properties
1. Gas generation: ≥215 ml/g;
2. Residue on sieve (38 μm mesh): ≤0.1%;
3. Average particle size: ≤12 (Dn) μm;
4. Decomposition temperature: 200-210°C;
5. Heating loss: ≤0.15%;
6. Ash content: ≤0.1%;
7. Purity (ADC): ≥97.0%
Storage
Store in a ventilated, cool, and dry place. Usage
Production Method
Urea oxidation method. Using urea, chlorine, and caustic soda as starting materials, hydrazine hydrate is first prepared. The obtained hydrazine hydrate reacts with urea under the action of sulfuric acid to form biurea, which is then oxidized with chlorine to produce ADC foaming agent. The product is obtained after washing, centrifugation, and drying.
Producing 1 ton of this product requires 1.9–2.2 tons of urea (N≥46%), 2 tons of sulfuric acid (98%), 2.0–2.3 tons of caustic soda (100% equivalent), 0.01 tons of sodium bromide, 1.7–1.9 tons of liquid chlorine (99.5%), and 0.1–0.11 tons of potassium permanganate.