China HY-9072 Aluminum-Magnesium Alloy Release Agent - China Supplier
China HY-9072 Aluminum-Magnesium Alloy Release Agent - China Supplier China HY-9072 Aluminum-Magnesium Alloy Release Agent - China Supplier China HY-9072 Aluminum-Magnesium Alloy Release Agent - China Supplier China HY-9072 Aluminum-Magnesium Alloy Release Agent - China Supplier

HY-9072 Aluminum-Magnesium Alloy Release Agent

Price:¥12.8 /kg
Industry Category: Chemicals
Product Category:
Brand:
Spec: HY-9072


Contact Info

Other Products

Description
Additional Information

HY-9072 Aluminum-Magnesium Alloy Release Agent

    Introduction:This product is a water-based release agent, classified as an environmentally friendly product. It is non-toxic, non-corrosive, diluted with alcohol solvents, and does not produce harmful fumes. It exhibits lubricity, oil solubility, wear resistance, defoaming properties, anti-adhesion, printability, isolation, and high-temperature resistance, and can be used directly. Through high-temperature film formation and lubrication, it ensures high whiteness of the cast surface after demolding, without yellowing or blackening, while effectively inhibiting carbon buildup on molds and extending their service life.



Parameters

Appearance: Milky white liquid

Solid content: 15~30% (depending on dilution ratio and cost-performance requirements)
pH value: 7.0-8.5
Temperature resistance range: 200-700°C
Applicable metals: Aluminum/Zinc/Magnesium alloys


Features

1. High temperature resistance, anti-carbon buildup
2. Strong mold protection capability
3. High precision density, oxidation resistance
4. Excellent release performance, suitable for aluminum/zinc alloys
5. High precision density, oxidation resistance


Usage Instructions

1. Dilution ratio
Dilute at 1:100 (concentrate:water), mix well before use. Using deionized water can improve anti-carbon buildup, anti-corrosion, and surface finish. Users should choose between tap water and deionized water based on practical results.
2. Spraying process
Mold temperature control: Preheat the mold to 150-200°C before spraying to ensure uniform film formation of the release agent;
Spraying equipment: Use an atomizing spray gun (pressure 0.3-0.5MPa), spray evenly from a distance of 20-30cm from the mold surface;
Spraying amount: Spray for 1-2 seconds per cycle to form a uniform transparent film layer.
3. Operation process
Mold cleaning → Preheating → Spraying release agent → Injecting molten metal → Cooling and demolding → Mold maintenance.


Shelf life: 12 months

Industry Category Chemicals
Product Category
Brand:
Spec: HY-9072
Stock:
Origin: China / Jiangsu / Wuxishi
About Toocle.com - Partner Programme - Old Version