Stainless Steel A507 Welding Electrode
Contact Info
- Add:河北省邢台市信都区永康街533号, Zip:
- Contact: 韩吉英
- Tel:13833921539
- Email:2891465062@qq.com
Other Products
GB/T 983 E16-25MoN-15
Suitable for welding low-alloy and medium-alloy steels in the quenched state, dissimilar steels, structures with high rigidity, and corresponding heat-resistant steels.
A Cr16Ni25Mo6 stainless steel electrode with a basic coating, featuring good welding process performance, stable arc, easy slag removal, and aesthetically pleasing weld formation.
Direct current reverse polarity (DC+).
Chemical Composition of Deposited Metal (%)
| Test Item | C | Mn | Si | P | S | Cr | Ni | Mo | Cu | N |
| GB/T Standard | ≤0.12 | 0.50~ 2.50 | ≤0.90 | ≤0.035 | ≤0.030 | 14.0~18.0 | 22.0~27.0 | 5.0~7.0 | ≤0.75 | ≥0.10 |
| Example Value | 0.055 | 1.65 | 0.34 | 0.020 | 0.007 | 15.85 | 24.45 | 5.90 | 0.11 | 0.13 |
Mechanical Properties of Deposited Metal
| Test Item | Rm (MPa) | A(%) |
| GB/T Standard | ≥610 | ≥30 |
| Example Value | 655 | 40 |
Reference Current
Electrode Specification (mm) | Φ2.5 | Φ3.2 | Φ4.0 | Φ5.0 | |
Welding Current (A) | Flat, Horizontal | 50~90 | 80~120 | 100~150 | 140~180 |
Vertical, Overhead | 60~80 | 90~110 | 110~140 | — | |
1. Drying Requirement: Electrodes must be baked at 250°C for 1 hour before use and used immediately after baking.
2. Use low current and short arc welding as much as possible during welding, with minimal oscillation amplitude.
| Industry Category | Machinery |
|---|---|
| Product Category | |
| Brand: | 金帝牌 |
| Spec: | 2.5/3.2/4.0/5.0mm |
| Stock: | 5000 |
| Manufacturer: | |
| Origin: | China / Hebei / Xingtaishi |