| Items | Specification | |
| Premium Grade Powder | First Grade Powder | |
| Visual Appearance | Dark-green Powder | |
| Initial Melting Point, ℃ min. | 86.00 | 83.00 |
| Heat Loss,% max. | 0.50 | 0.50 |
| Nickel content,% | 12.0-13.0 | 11.8-12.8 |
| Density,g/cm³ | 1.26 | 1.26 |
| Residue on 150µm,% max. | 0.10 | 0.10 |
| Residue on 63µm,% max. | 0.50 | 0.50 |
| Additive,% | - | 1.0-2.0 |
Properties: Antioxidant Safflower® NDBC is a dark-green powder.
Density: 1.26g/cm³. Flash point: 260°C.
Soluble in chloroform, benzene and carbon disulfide, slightly soluble in acetone,
insoluble in water.
Uses: Mainly used in synthetic rubbers such as styrene-butadiene rubber, chloroprene rubber and chlorosulfonated polyethylene.
It can prevent rubber from cracking caused by sunlight and ozone, and improve the heat resistance of chloroprene rubber and chlorosulfonated polyethylene.
It is used as a light stabilizer and antiozonant for polymer materials in the plastic industry. It has excellent stabilizing effect when used in polypropylene fibers, films and narrow tapes, but will make the products yellowish-green. The dosage is 0.3~0.5%. For applications in rubber products that come into contact with food, please refer to the regulations in the relevant chapters of BgVV.
Safety and Toxicity: Please refer to the relevant Material Safety Data Sheet (MSDS).
Storage: Store in a sealed, cool, dry and well-ventilated place. Avoid direct sunlight.
Improve the heat resistance of chloroprene rubber and chlorosulfonated polyethylene.